NRU GmbH

NRU GmbH

Südstraße 3
D-09221 Neukirchen
Deutschland
Email: info(at)nru-gmbh.de
WWW: www.nru-gmbh.de
Phone: +49 371 28155-0
Fax: +49 371 28155-20





The casting of metal into lost ceramic forms is one of our core competences. We are able to use almost all casting alloys, or we can do even own charges. Numerous steels, alloys based on nickel or cobalt as well as copper, titanium, aluminum or zinc alloys can be cast in NRU. As lost models, we have printed PMMA or wax models available. With the help of our automated robotic shell production, we can flexibly realize batch sizes from the single piece up to a series of 1000 castings with a mass of one gram to 6 kg.