Binder Dosing Systems


This is an especially equipment for exactly dosing chemical binders for foundry sands (datec Dosier- und Automationstechnik GmbH). The design is simple and robust.


Features:

• volumetric dosing independent of binder viscosity
• guaranteed repetitive accuracy +/- 0.5 %
• The bellow dosing equipment is absolutely maintenance-free.
• The desired dosing volume is easily adjustable by:

a) manually infinitely adjustable set screw
b) selection of two binder quantities using selector switches
c) infinite adjustment of dosed quantity

Figure 1 shows an example KLEIN Anlagenbau AG
Figure 2 Foseco Foundry Division Vesuvius GmbH, Binder Dosing Systems

  • Fig. 1: Binder Dosing System BDG (KLEIN Anlagenbau AG)
  • Figure 2 Foseco Foundry Division Vesuvius GmbH, Binder Dosing Systems