Core gumming jig

Equipment for ensuring precise dimensional accuracy when assembling the core (s. Core assembly).

If the stability of partial cores is rather low or it is not possible to correctly fix a partial core in its position, a core gumming jig is required. The core will rest on the jig until the gumming adhesive has hardened (s. Hardening).