Die cavity-filling phase

Second phase of the casting process between the pre-filling phase and the holding pressure phase.

The mold filling phase describes the actual casting process, in which the melt is pressed into the mold with high piston speeds of up to 6 m / s. This results in very short mold filling times in the range of a few milliseconds. In this phase, virtually no venting is possible.