Melting point of the eutectic.
The eutectic temperature of iron-carbon materials is 1147 °C in the meta-stable system along the E-F line, with C contents of 2.06 - 6.67 %; the eutectic spot C has a C content of 4.30 % for the meta-stable system (s. a. Iron-carbon phase diagram).