Injector

Equipment for the direct injection of solid substances into molten material using inert carrier gas.

Among others, injectors are used to chargecarburization agents and desulphurization agents to molten cast iron and steel as well as to deoxidize and micro-alloy steel, to remove silicon, phosphor and sulfur from pig iron and to inject additives into other molten metals without any major losses.
 