Plant used to produce magnesium castings with the low pressure gravity die casting process.
In this new process, the mold is filled by a mechanical melt pump
(Fig. 1) as the conventional low pressure gravity die casting process with gas pressurization (e.g. for aluminum alloys) is not very suitable for magnesium. The pump is controlled via pressure or time measurement so that the mold can be filled in the desired way - also with different filling speeds.
These leads to the following advantages compared to conventional pressurization with gas:
While the melt solidifies in the mold, the shrinkage is compensated for by the final pressure of the melt pump. For particularly long solidification times - e.g. for thick-walled castings - the final pressure can also be applied using a specially designed cylinder with pistons. This process, for which a patent application has been submitted, enables the feeding of the melt into the form by the pump to be blocked by pushing the pistons forward and the desired final pressure to be created with the pistons.
Additional references:
Low pressure casting plant
Magnesium melting and dosing furnace