Mold part

Main components of a casting mold.

Two-part molds comprise of cope and drag, also referred to as mold top and mold bottom, i.e. two mold parts or mold halves. Three- or multi-part molds comprise additional mold parts. Moreover, according to the type of mold, differentiation is made between box mold parts, boxless mold parts, and core mold parts. 

 

 