Multi airpipe sensor system

Compact sensor for die casting processes (Fig. 1) which enables measurements of up to four parameters through the vacuum supply of the die casting mold, such as:

The sensor can be mounted behind a washboard or behind a vacuum valve block, the installation positions as well as the characteristic curves of separate sensors are illustrated in Fig. 2.

Additional references:

Vacuum sensor
Mold filling control sensor
Mold cavity pressure sensor
Metal front temperature sensor
metal front contact sensor
Air flow sensor
Humidity sensor
Residual gas sensor





  • Fig. 1: Electronics GmbHmulti airpipe sensor system (MASS)
  • Fig. 2: Sensor signal curves of the multi airpipe sensor system (MASS) during the injection process, Source: Electronics GmbH1) Ventilated mold2) High gas portion3) Low gas portion