Output

Casting weight percentage of the total pouring weight, with the pouring weight being the overall weight of the poured metal, including risers and gating system. The following simplified equation shall apply (Eq. 1):

Eq. 1

Accordingly in alloying, the added alloy element proportion actually present in the finished alloy material in relation to the total charge of alloy additives is also referred to as output.