Alloyed structural stainless steel, e.g. with material number 1.3401 (PANTANX 3401) and also the term for wear-resistant, white chromium cast iron with a standard composition of
2,4% C
0.8% Si
1.2% Mn
26% Cr
1.2% Mo
0.5% V.
The casting material is used for the production of wear-resistant pipes in the composite centrifugal casting process.