Material reclaimed after successful reclamation.
Foundry sands, both mono systems and combined systems, are reclaimed to an increasing extent. After the binder residues (bentonite, resin) have been removed, the reclaimed material is supplied to the process as new sand replacement (s. a. New sand addition) at a certain rate. (s. a. Sand reclamation)
Additional references:
Reclaimed material yield, Reclamation, Reclamation rate