Scale of hardness

Classification of 10 levels of increasing hardness to compare mineral substances according to Mohs on the basis of Vickers hardness HV:

1.     Talk             --
2.     Gips             36
3.     Kalkspat     140
4.     Flußspat     190
5.     Apatit          540
6.     Feldspat     600 – 750
7.     Quarz         900 – 1280
8.     Topas         1430
9.     Korund        1800
10.   Diamant      10000