Solidus line

Line in the phase diagram of an alloy system (Fig. 1) connecting all solidus temperatures and delimiting the temperature range in which the melt is only present in the solid state.

Additional references:
Solidification interval
Liquidus line
Liquidus temperature

  • Fig. 1: Solidus line in the Al-Si system (up to 20% Si)