TBM process

In addition to oxygen, argon or nitrogen is blown in through the nozzle bricks at the bottom of the basic oxygen steel converter.

The advantages of this process are the improved stirring of the melt, shorter blowing periods, lower oxygen consumption and the longer service life of the refractory brick lining. Moreover, this process improves overall steel quality and allows for a wider production range of steel types.