Cavity sensor for die casting processes (Fig. 1) which is built in the vacuum supply leading to the die cast mold and which records the amount of air during evacuation (negative pressure sensor).
A characteristic pressure and/or negative pressure cirve during mold evacuation is shown in Fig. 1.
Additional references:
Vacuum-assisted die casting
Multi.stage vacuum process
Vacural process
Mold filling control sensor
Mold cavity pressure sensor
Metal front temperature sensor
Metal front contact sensor
Multi airpipe sensor system
Air flow sensor
Humidity sensor
Residual gas sensor