apromace

Quality assurance through the use of the thermal analysis package apromaceTA

The thermal analysis provides information on the metallurgical behavior of molten metal.

 

Source: apromace

As a method for determining the characteristic points (POI) during the phase transformations from the cooling curve or heating curves of a melt, the thermal analysis serves as a control element of the process control in foundries.

With the apromaceTA thermal analysis package, quality-relevant parameters are recorded and evaluated during production, so that it is possible to influence the metallurgical state of liquid metals in a timely manner in which deviations are diagnosed and corrected by controlling the proportion of the melting components.

Source: apromace