Bending Strength molding materials
Source: bindur.de
The binder PUROLiT consists of two components (resin and hardener). Its reaction rate is controlled by a catalyst. Our binding agent is almost odorless, low in emissions and therefore safe to handle. In addition to the processing-friendly characteristics, it shows a high stability.
Eligible studies of established laboratories show that the environmentally benign properties, qualify the discharged core sands, in accordance to the landfill ordinance, as non-hazardous waste.
We have the first powerful organic binding agent available that is designed to cater for safe and cost-effective foundry operation.
Source: bindur.de