Source: EBNER
Hazelett joins EBNER GROUP - Hazelett Strip-Casting Corporation of Colchester, Vermont USA has become a member of the EBNER GROUP, headquartered in Leonding, Austria, through the acquisition by EBNER of a majority interest in Hazelett.
Mino S.p.A, based in Alessandria, Italy will remain a shareholder along with David Hazelett, who will also remain as both a shareholder and President. The EBNER GROUP consists of EBNER Industrieofenbau in Leonding, Austria, EBNER Furnaces in Wadsworth, USA, EBNER Industrial Furnaces in Taicang, China, Gautschi Engineering in Ranshofen, Austria, HPI in Ranshofen, Austria, GNA alutech in Montreal, Canada, and EED in Taicang, China. Together the companies offer a wide range of furnace facilities, upstream and downstream auxiliary equipment, project management and services to the aluminum, steel and copper base metals sectors.
Together with Mino, the EBNER GROUP will be able to offer complete process lines to the aluminum flat rolled products industry featuring Hazelett twin-belt continuous casting technology.
Hazelett technology is used in metal manufacturing processes worldwide to cast aluminum, copper, zinc, and lead into metal strip and bar used to create countless products. Hazelett has been a leader in the design and manufacture of continuous casting machines for the global metal industries for over 100 years. Similarly, EBNER has been a leader in the design and manufacture of thermal processing furnaces for over 70 years. Both have been family-owned throughout their histories and this merger preserves that legacy.
Source: EBNER