The individual mounted impact blades are made of very resistant powder-metallurgical tool steel and guarantee maximum service life. The castings are brought to the rotating knock-off wheel by means of a robot or a manipulator. Depending on the design of the gripper, all sides of the casting can thus be freed from burrs, sprues, pins, etc. A robot-guided deburring wheel can also be implemented. Pre-deburring of the components also increases the service life of the possible subsequent grinding process, as the result is a constantly constant residual burr height. Depending on the thickness of the burrs, the deburring wheel can also take over complete deburring and replace the grinding process step.
Source: FILL
ADVANTAGES
- High flexibility
- Deburring of castings "in the black"
- Long service lives
- Low tool costs
- Burrs up to 100 mm in height can be removed.
- Low investment costs