GIFA 2019, the most important trade fair in the world for the foundry industry will be held on 25-29 June 2019 in Düsseldorf, Germany. Together with the with GIFA Forum, this represents an ideal opportunity to get an overview of the latest trends and technology developments for the foundry industry. At the Foseco booth, visitors will discover new, innovative solutions for iron, steel and nonferrous foundries. We look forward to seeing you on our stand in Hall 12 Stand no. 12A01.

 

Feeding Systems for Iron and Steel Foundries

The application of feeder sleeves is a major factor in reducing metal remelt and fettling costs in foundry customers. By working in close partnership with foundries, Foseco continues to deliver tailored solutions for specific applications and develop new process technologies.

In this year’s exhibition, we will showcase several new developments that advance the capabilities of the foundryman in optimising casting yield, minimising defects and reducing production costs.

The new range of FEEDEK VAK spot feeders will be presented through a variety of ductile iron castings. This patented development provides an improved feeder neck pass-through on the most critical feeding applications.

Figure: Foseco’s new, patented FEEDEX VAK feeding technology

The development of FEEDEX SCK (Sleeve Construction Kit) feeders opens up the application of spot feeding to the jobbing iron and steel sector where the modular product range enables our customers to optimise both casting yield and fettling costs on large steel and iron castings.

All relevant exhibits will feature simulations using the most recent version of the Foseco Pro Module for MAGMASOFT.