More and more automobile manufacturers are requesting that direct part markings be made right at the extraction of the casting from the die, thereby ensuring complete traceability throughout the entire value chain.

Information is encoded and engraved on the parts using protocols, such as the one used by Data Matrix Codes.
Read full technical paper here

Source:Laserax