Melting base

Foundry-specific expression for a melt that is used for magnesium treatment, and therefore for production of nodular graphite cast iron (GJS). For standardization of the chemical composition of this melt, particularly for standardization of the silicon content, it must be taken into account whether a Mg pre-alloy or pure magnesium is used for the process.