Nowadays usually a digital picture of the structure of a metallographic specimen viewed under the microscope. The magnification used and if possible also the kind of metallographic specimen preparation, e.g. unetched or etched, must be indicated in any case. For the sake of completeness, the type of microscope (microscope, macroscope, REM) should also be indicated.