Order check list

The check lists illustrated in tables 1 to 4 contain the most important information with regard to the various items that must or may be agreed between the purchaser and the manufacturerund at the time of acceptance of orders.

The check lists represent the aspects specified in sub-sections and paragraphs of European standard EN 1559-1:1997.

Literature references:
DIN-Taschenbuch 452, Aluminium: Normen, Hüttenaluminium, Aluminiumguss, Schmiedestücke, Vormaterial - Normen, Editor: DIN Deutsches Institut für Normung e.V., Beuth Verlag GmbH
ISBN 3-410-14103-0

  • Table 1: Binding and optional information to be specified by the purchaser
  • Table 2: Optional information for manufacturing
  • Table 3: Information on the requirements for the cast part
  • Table 4: Information for definition of inspection and identification characteristics